JIS G3115 SPV355 Pressure Vessel Steel Plate

JIS G3115 SPV355 Pressure Vessel Steel Plate

SPV355 steel is a Japanese Standard (JIS G3115) pressure vessel steel known for good weldability and suitability for intermediate temperature service, featuring a minimum yield strength of 355 MPa (for certain thicknesses) and used in boilers, heat exchangers, and tanks. It offers excellent strength, impact resistance, and ductility, with common applications in petrochemical, energy, and general manufacturing for components like reactors, storage tanks, and high-pressure pipes.
Envoyez demande
Discuter maintenant
Description
Paramètres techniques

SPV355 steel plate is for pressure vessels for intermediate temperature service in JIS G3115-2000 SPV355 Grade has a good weldable and used in high temperature equipment and pressure vessel.JIS G3115 specifies the hot-rolled steel plates with improved weldability to be used for pressure vessels,equipments for high pressure service(excluding those to be used for high temperature and low temperature services). SPV355 steel plates are widely used in the fabrication of boilers and pressure vessels in industries such as petrochemical and manufacturing.

 

SPV355Chemical Composition

C

P

S

SPV355

0.20

0.55

1.60

0.030

0.030

Carbon Equivalent: Ceq=【C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15】%

 

 

SPV355 Mechanical Property

SPV355

6-50

355

490-610

14%

50-100

355

490-610

18%

100-200

315

490-610

21%

 

Technical Requirements & Additional Services for SPV355 steel plate:



♦ Ultrasonic test under EN 10160,ASTM A435,A577,A578
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2

 

JIS G3115 SPV355 Pressure Vessel Steel Plate

 

JIS G3115 SPV355 Steel Plate

A:We accept FOB,CIF,CFR and other international shipping terms.Port of loading can be specified according to customer requirements.

Q:Do you have after-sales service?

A:Of course, you can contact us at any time.we promise our products are all qualified. If you find any products are not qualified and unsatisfied your require,please contact us at any time.

 

étiquette à chaud: jis g3115 spv355 pressure vessel steel plate, China jis g3115 spv355 pressure vessel steel plate manufacturers, suppliers, factory, Navire de pression en acier au carbone, JIS G3193 ACTEUL, Navire de pression en acier doux, Plaque d'acier PVQ, SB450 Acier de la chaudière, Plaque en acier SPV235