Gneesteel is specialized in supplying EN10028-6 steel plate in P460QL1. For more information of P460QL1 steel plates, please check them in following:
Mechnical property for P460QL1 steel plate
| P460QL1 | <= 50 | > 50 <= 100 | > 100 |
| 460 | 440 | 400 | |
| <= 100 | > 100 | ||
| 550-720 | 500-670 | ||
Technical Requirements & Additional Services for P460QL1 steel plate:
♦ Simulated post-welded heat treatment (PWHT)
♦ Ultrasonic test under EN 10160,ASTM A435,A577,A578
♦ Issued Orginal Mill test certificate under EN 10204 FORMAT 3.1/3.2


GNEE have served clients in over 50 countries (North America, Europe, Southeast Asia, the Middle East, etc.) and gained rich experience in international trade terms (FOB, CIF, EXW) and local market requirements. Our efficient communication (English, Spanish, Arabic support) and transparent business processes make cooperation smooth and hassle-free.
étiquette à chaud: en10028-6 p460ql1 pressure vessel steel plate, China en10028-6 p460ql1 pressure vessel steel plate manufacturers, suppliers, factory, Plaques de chaudière à chaudière à chaud 16MO3, Plaques de qualité de la chaudière, P355NL1 P355NL2 Plaque en acier de la chaudière, P420ml2, P460NL1 P460NL2 Plaques d'acier de qualité de la chaudière, navire de pression en acier inoxydable